厂家(产地):Lubrizol 牌号:2102 销售方式:品牌经销 加工级别:注塑级 特性级别:增韧级 用途级别:通用级
产品特点

路博润ESTANE 2102-80A,耐油高回弹TPU Technical Data Sheet Type: Estane? 2102-80A is a thermoplastic polyurethane elastomer. Feature: Low compression set. 1 Typical properties; not to be construed as sales specifications. Fabrication conditions, part design, additives, processing aids, finishing materials and use conditions can all affect the integrity, performance and regulatory status of finished goods. 2 Tests conducted on 0.126 inch (3.2mm) injection molded specimen, unannealed, unless noted. Properties Test Method English S.I. Valuest Units Valuest Units Physical(1) Shore Hardness ASTM D 2240 84 A 84 A Specific Grity ASTM D 792 1.18 1.18 Taber Abrasion Resistance, 1000g, 1000 cycles; H-22 wheel (coarser) ASTM D 1044 - mg 10 mg Mold Shrinkage, Transverse direction ASTM D 955 -0.2-0.5 % -0.2-0.5 % Mold Shrinkage, Flow direction ASTM D 955 0.4-0.6 % 0.4-0.6 % Mechanical(2) Tensile Modulus -50% elongation - elongation -300% elongation ASTM D 412 560 800 1900 psi psi psi 3.9 5.5 13.1 MPa MPa Mpa Ultimate Elongation ASTM D 412 575 % 575 % Ultimate Tensile Strength ASTM D 412 5800 psi 40 Mpa Elongation Set After Break ASTM D 412 50 % 50 % Tear Strength, Die C ASTM D 624 600 PLI 105 KN/m Compression Set, Method B -22 hrs @ 25° C -22 hrs @ 70° C ASTM D 395 28 28 % % 28 28 % % Thermal Vicat Softening Point (120° C/hr, 9.8N) ASTM D 1525 185 o F 85.0 o C Glass Transition Temperature DSC -40 o F -40 o C CLTE, in-flow ASTM D 696 87.7 in/in/ o F 158 mm/mm/o C Processing Conditions (Typical) Drying Temperature (air dew point <-40C) 180-200 o F 82-93 o C Melt Temperature (Molding) 390-420 o F 199-216 o C Mold Temperature 60-140 o F 16-60 o

产品实拍
相关产品推荐